Effect of Atomization Gas Temperature on Powder Characteristics of CoCrMoW and NiCrMo Alloys for Dental Additive Manufacturing
MSE 2026 Materials Science and Engineering Congress, Darmstadt, Almanya, 29 Eylül - 01 Ekim 2026, ss.916, (Tam Metin Bildiri)
- Yayın Türü: Bildiri / Tam Metin Bildiri
- Basıldığı Şehir: Darmstadt
- Basıldığı Ülke: Almanya
- Sayfa Sayıları: ss.916
- Dokuz Eylül Üniversitesi Adresli: Evet
Özet
CoCrMoW and NiCrMo powders in the 15–45 μm range are widely used in dental additive manufacturing. This study examined the association between atomizing gas temperature and the yield and characteristics of both alloy powders. Each alloy was atomized industrially with unheated nitrogen (~24 °C) and with nitrogen preheated to nominal inlet temperatures of 100 and 200 °C, while all other process parameters were kept constant within each alloy. The powders were characterized by laser diffraction, SEM, Hall flow testing, apparent and tap density measurements, inert-gas fusion analysis, and XRD. Relative to the unheated condition, the normalized yield index of the 15–45 μm fraction increased to 104 and 125 for NiCrMo and to approximately 110 for CoCrMoW at 100 and 200 °C, respectively. NiCrMo atomized at 200 °C showed the broadest particle-size distribution, the highest fraction below 15 μm, and the highest nitrogen content, whereas CoCrMoW remained comparatively stable. All powders were near-spherical and showed dominant FCC reflections. As each condition was represented by a single run, the results are descriptive. Gas preheating may increase the target-fraction yield, particularly for NiCrMo, but optimization should also consider particle-size distribution, nitrogen uptake, flowability, and L-PBF performance.