AN INVESTIGATION OF THE MECHANISM OF THERMALLY ACTIVATED DEFORMATION IN CERTAIN NI-AL-TA AND NI-AL-HF SUPERALLOYS
PHYSICA STATUS SOLIDI A-APPLIED RESEARCH, vol.83, no.2, pp.507-511, 1984 (SCI-Expanded)